Customization: | Available |
---|---|
Type: | Clay Wet Sand |
Casting Method: | Thermal Gravity Casting |
Still deciding? Get samples of US$ 3.8/kg
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
1.Material Grade: AS 2027 Cr35;
2.Size: drawings
3.Process: Sand Casting;
4.Hardness: HRC33-43;
5.Suface Finish: Ra.100;
6.The size tolerance: As per CT13;
7.Application: Mine,Ball,SAG and Cement Mill;
8.Package: Packed by steel crates
9.Chemical Composition:
Reference Standard (ISO 21988-2005) |
Nominal Chemical Composition (W%) | Eqv. Standards | |||||||||
C | Si | Mn | Ni | Cr | Mo | Cu | P | S | |||
ISO 21988/JN/ HBW600XCr35 |
3.0-5.5 | ≤1.0 | 1.0-3.0 | ≤1.0 | 30.0-40.0 | ≤1.5 | ≤1.2 | ≤0.06 | ≤0.06 | AS 2027 Cr35 |