Standard Specification for High Cr Abrasion-resistant White Iron
Reference Standard |
Nominal Chemical Composition (W%) |
Eqv. Standards |
||||||||
|
C |
Si |
Mn |
Ni |
Cr |
Mo |
Cu |
P |
S |
|
ISO 21988/JN/ |
1.8-3.6 |
≤1.0 |
0.5-1.5 |
≤2.0 |
11.0-14.0 |
≤3.0 |
≤1.2 |
≤0.08 |
≤0.08 |
EN-GJN-HV600(XCr11) |
ISO 21988/JN/ |
1.8-3.6 |
≤1.0 |
0.5-1.5 |
≤2.0 |
14.0-18.0 |
≤3.0 |
≤1.2 |
≤0.08 |
≤0.08 |
EN-GJN-HV600(XCr14) |
ISO 21988/JN/ |
1.8-3.6 |
≤1.0 |
0.5-1.5 |
≤2.0 |
18.0-23.00 |
≤3.0 |
≤1.2 |
≤0.08 |
≤0.08 |
EN-GJN-HV600(XCr18) |
ISO 21988/JN/ |
1.8-3.6 |
≤1.0 |
0.5-2.0 |
≤2.0 |
23.0-30.0 |
≤3.0 |
≤1.2 |
≤0.08 |
≤0.08 |
EN-GJN-HV600(XCr23) |
ISO 21988/JN/ |
3.0-5.5 |
≤1.0 |
1.0-3.0 |
≤1.0 |
30.0-40.0 |
≤1.5 |
≤1.2 |
≤0.06 |
≤0.06 |
AS 2027 Cr35 |
ISO 21988/JN/ |
2.6-2.9 |
≤1.0 |
≤1.0 |
≤1.0 |
18.0-21.0 |
1.4-2.0 |
0.8-1.2 |
≤0.06 |
≤0.06 |
AS 2027 CrMoCu 20 2 1 |
Special Features:
1.We adopt Sand Cast Process to make High Cr & Ni hard chute liners;
2.We do quenching & tempering treatment for high Cr & Ni hard white iron plates to achieve high hardness.
3. Cr15Mo3 castings: more than HRC56; AS2027 Cr27 castings: more than HRC59; Ni-hard white iron: more than HRC54.
· Shell Liners for the First Chamber ,the Second Chamber,the Third Chamber;
· Lifting Liners
· Step Liners
· Wave Liners
· Corrugated Liners
· Inter End Liners
· Inter mediated Diaphragm Liners(Grate Liners,Blind Liners)
· Outlet End Liners